Wet, sticky feed and high tonnage throughput break ordinary panels quickly — and blind them even faster. This 40mm-thick polyurethane panel is cut and moulded to your deck dimensions in a hydrolysis-resistant wear compound, with an aperture layout engineered to keep the surface open right through the shift.
What this panel is built to do
Recommended applications
Coal preparation and washing decks · wet sand and gravel screening · dewatering and drain sections · mobile plant decks running high-moisture feed — anywhere standard panels peg, blind or wear through within weeks.
Technical data
| Item | Specification |
|---|---|
| Thickness | 40 mm standard; 25–60 mm on request |
| Panel size | Custom cut to your deck drawing |
| Aperture | 3–100 mm, slotted or square; tapered option |
| Hardness | Shore A 85 (75–95 available) |
| Compound | Hydrolysis-resistant wear grade polyurethane |
| Density | 1.10–1.15 g/cm³ |
| Tensile strength | ≥ 30 MPa |
| Tear strength | ≥ 80 kN/m |
| Abrasion (DIN 53516) | ≤ 40 mm³ |
| Rebound resilience | ≥ 40 % |
| Service temperature | −30 °C to +80 °C |
| Fixing | Pin and sleeve, bolt-through, or rail clamp |
Ordering
Send deck dimensions, screen motion (stroke and speed), feed moisture and cut point. We return a dimensioned drawing for your approval, and grade aperture size and panel thickness deck position by deck position — feed end through to discharge — before production starts.
FAQ
What thickness should I use on my deck?40 mm suits the feed end, where drop height and lump size are highest. Thinner sections of 25–30 mm are often enough on the middle and discharge sections, which cuts weight and cost without shortening panel life. We specify thickness per deck position rather than one thickness across the whole machine.
Can you fit my existing frame without drilling?Yes. Send a drawing or a measurement sheet with fixing centres, and the fixing positions are moulded to match your current frame. No deck drilling and no modification on site.
Will these panels peg in sticky, wet feed?The tapered slot opens through the thickness of the panel, so near-size particles release on the return stroke instead of wedging. Combined with panel flex under vibration, this is what keeps the deck open in high-moisture circuits where square-hole rubber panels blind.
What is your MOQ and lead time?MOQ: 10 pcs. Standard lead time: 15 days. Standard mold making: 10 days.