Quick Link
Quick Contact
Address
No.367 Beijing Road, Longquanyi District, Chengdu, China
Tel
86--13981727059
Our Newsletter
Subscribe to our newsletter for discounts and more.
Industrial minerals are sold on properties that a screen can quietly destroy. Kaolin is sold on brightness and particle size. Bentonite is sold on swelling behaviour. Talc is sold on purity and platelet structure. In each case the value sits in specifications that are measured after the screen, which means the panel's job is to make a cut without changing anything else about the material.
Fine cuts held in slurry. Kaolin and bentonite are usually screened wet, at solids contents where the material behaves as a slurry rather than as particles. A moulded slot keeps its width under continuous wet duty, so the cut point stays where it was specified instead of drifting coarser through a campaign.
Bentonite swells and grips. Bentonite takes on water and becomes genuinely adhesive, which is the hardest case on this list. The tapered aperture plus the flex of the panel under vibration is what keeps the surface working; a rigid panel with square holes simply fills.
No metal in the wear surface. Kaolin and talc are graded on brightness, and iron staining from steel media is a real product defect, not a cosmetic one. A moulded polyurethane panel has no wire to shed and no rust to contribute.
Abrasion from the quartz fraction. Kaolin deposits carry quartz sand, and that fraction does the cutting regardless of how soft the clay is. A wear grade compound at ≤40 mm³ DIN abrasion holds the land width between apertures, which is what keeps the cut stable.
Where it runsKaolin wet classification and degritting, bentonite screening and sizing, talc and soapstone grading, industrial mineral slurry screening, and classification ahead of thickening, filtration or drying.
Technical data| Item | Specification |
|---|---|
| Thickness | 40 mm standard; 25–60 mm on request |
| Panel size | Custom cut to your deck drawing |
| Aperture | 3–100 mm, slotted or square; tapered option |
| Hardness | Shore A 85 (75–95 available) |
| Compound | Hydrolysis-resistant wear grade polyurethane |
| Density | 1.10–1.15 g/cm³ |
| Tensile strength | ≥ 30 MPa |
| Tear strength | ≥ 80 kN/m |
| Abrasion (DIN 53516) | ≤ 40 mm³ |
| Rebound resilience | ≥ 40 % |
| Service temperature | −30 °C to +80 °C |
| Fixing | Pin and sleeve, bolt-through, or rail clamp |
Send mineral type, solids content, cut point, screen motion and the specification you have to meet. For kaolin, tell us the quartz content — it decides section thickness and compound more than tonnage does.