Impact Screen Panel in Polyurethane for High Drop Height Feed Points
Most screen media is selected on tonnage and aperture, and then fails for a reason nobody specified: the drop height at the feed point. A 2 m fall onto a deck turns a 300 mm lump into a hammer. The panel takes that hit several thousand times a shift, in the same place, and a plain moulded section eventually cracks at the point of contact or works loose at the nearest fixing.
Energy absorbed, not returned. Polyurethane with rebound resilience at or above 40 % deforms under the hit and recovers. That is what stops the crack initiating, and it is why the panel survives impact that would dent a steel plate permanently.
Steel frame spreads the point load. A lump lands on perhaps 200 mm² of surface. Without a frame, that load goes straight into the panel body locally and into the nearest fixing. With an encapsulated frame, it is distributed across the panel and into the support rails, so no single fixing sees the whole hit.
Wide lands at the impact zone. The feed-end section is specified with wider lands between apertures — less open area in the first 300–500 mm, where the material is still moving fast and the bed is thin, and full open area from there on. Open area at the impact point buys nothing; strength buys service life.
Replaceable in sections. Impact damage is local. Because panels are cut to your deck drawing, the feed-end row can be specified as its own panel size, so a damaged section is replaced on its own rather than as a full deck set.
Where it runs
Feed points of primary and secondary screens, transfer chute discharge, crusher discharge decks, loader-fed mobile plants and any deck with a drop height above about 800 mm.
Technical data
| Item | Specification |
| Thickness | 40 mm standard; 25–60 mm on request |
| Panel size | Custom cut to your deck drawing |
| Aperture | 3–100 mm, slotted or square; tapered option |
| Hardness | Shore A 85 (75–95 available) |
| Compound | Hydrolysis-resistant wear grade polyurethane |
| Density | 1.10–1.15 g/cm³ |
| Tensile strength | ≥ 30 MPa |
| Tear strength | ≥ 80 kN/m |
| Abrasion (DIN 53516) | ≤ 40 mm³ |
| Rebound resilience | ≥ 40 % |
| Service temperature | −30 °C to +80 °C |
| Fixing | Pin and sleeve, bolt-through, or rail clamp |
Ordering
Send drop height, maximum lump size, feed rate and deck drawing. Where the drop is very high, we will also ask about the chute — a chain curtain or a rock box upstream often costs less than another 20 mm of panel.