Wear Resistant Scalping Screen Mesh Polyurethane Screen Panel

Place of Origin: Chengdu, China
Brand Name: Zhicheng Screen
Certification: ISO 9001:2015
Model Number: ZC-PU-WR42
Minimum Order Quantity: 10 Pieces
Price: USD 22-48 / Piece
Packaging Details: Export-grade wooden pallet with stretch film and shock-proof foam
Delivery Time: 7-15 days for stock, 20-30 days for production
Payment Terms: T/T,L/C
Supply Ability: 5000 Pieces per Month
Inquiry Now
Get A Quote
Specifications
Highlight Features

Wear Resistant Scalping Screen Mesh

,

Wear Resistant Polyurethane Screen Panel

,

Scalping Screen Mesh Polyurethane

Material:
Imported High Wear-Resistant Polyurethane
Open Area:
32% - 42%
Service Life:
6-12 Months
Min Aperture:
3 Mm
Structure:
Embedded Metal Skeleton
Hole Design:
Cone-shaped, Anti-clogging
Application:
Coal, Iron Ore, Zinc Ore Separation
Product Description

Scalping Screen Panel in Polyurethane for Duty After the Primary Crusher

Scalping is the least forgiving screening job on a plant. The feed comes straight from a jaw or gyratory, it is coarse, it is sharp, and it arrives in surges rather than at a steady rate. Everything downstream depends on this deck doing its job — if the scalping screen blinds or breaks, the secondary crusher gets flooded and the whole circuit slows down.

Built for surge loading. A scalper sees the peak, not the average. Panels are specified with the frame carrying structural load so that a surge of coarse rock does not deflect the deck into the support rails or work the fixings loose.

Sharp edges, not round particles. Crushed rock has edges, and edges cut. A compound with tear strength at or above 80 kN/m resists the cutting action that opens up a slot or splits a land, which is the dominant wear mechanism on scalping duty.

Aperture that holds the cut. The scalping cut point sets the load on the secondary crusher. If the aperture wears open by 5 mm over a campaign, the secondary gets more fines it did not need and the circuit loses capacity. A moulded polyurethane aperture holds its dimension far longer than rubber or punched plate.

Section sized by drop height. Feed-end rows at 40 mm, downstream at 25–30 mm. On most scalpers this reduces total panel mass by a third against an all-40 mm deck, with no loss of life where the bed is thin.

Where it runs

Scalping ahead of secondary and tertiary crushers, run-of-mine screening at the pit, C&D material ahead of a jaw, and slag or clinker handling where the feed is coarse and hot-material risk is absent.

Technical data

Item

Specification

Thickness

40 mm standard; 25–60 mm on request

Panel size

Custom cut to your deck drawing

Aperture

3–100 mm, slotted or square; tapered option

Hardness

Shore A 85 (75–95 available)

Compound

Hydrolysis-resistant wear grade polyurethane

Density

1.10–1.15 g/cm³

Tensile strength

≥ 30 MPa

Tear strength

≥ 80 kN/m

Abrasion (DIN 53516)

≤ 40 mm³

Rebound resilience

≥ 40 %

Service temperature

−30 °C to +80 °C

Fixing

Pin and sleeve, bolt-through, or rail clamp

Ordering

Send crusher setting (CSS), maximum lump size, feed rate, deck drawing and drop height. The CSS and the scalping cut point have to be consistent; if they are not, we will flag it before quoting.