Grizzly Screen Panel in Polyurethane as a Bar and Rod Deck Replacement
A bar grizzly has two costs that never appear on the purchase order: the bars wear and have to be replaced one by one, and every bar replacement means a deck shutdown. On a plant where the grizzly is doing primary scalping, that is a maintenance item that arrives more often than anyone plans for.
A deck that is replaced as panels, not bars. Instead of 30 individual bars welded or bolted in place, the deck is a set of panels with moulded apertures. A worn section is one panel, changed in minutes, rather than a cutting and welding job on the deck.
Non-blinding at coarse sizes. Bar decks are prone to wedging, because a bar has no taper and a near-size lump sits on it until someone bars it off. Tapered moulded apertures release that material, which keeps the deck working through a wet or sticky feed.
Lighter than a bar deck. A bar grizzly is heavy by construction — thick bars on a steel frame. A polyurethane panel deck delivers the same aperture at a fraction of the mass, which reduces load on the screen frame and makes the deck easier to inspect.
No bar flutter. Individual bars vibrate independently, and that flutter is what wears the mounting points and eventually cracks them. A panel moves as one piece, so there is nothing to work loose individually.
Where it runs
Primary scalping ahead of a jaw crusher, run-of-mine separation, skip and tip receiving decks, and coarse waste separation where a bar grizzly is currently in service.
Technical data
|
Item |
Specification |
|
Thickness |
40mm standard; 25–60 mm on request |
|
Panel size |
Custom cut to your deck drawing |
|
Aperture |
3–100 mm, slotted or square; tapered option |
|
Hardness |
Shore A 85 (75–95 available) |
|
Compound |
Hydrolysis-resistant wear grade polyurethane |
|
Density |
1.10–1.15 g/cm³ |
|
Tensile strength |
≥ 30 MPa |
|
Tear strength |
≥ 80 kN/m |
|
Abrasion (DIN 53516) |
≤ 40 mm³ |
|
Rebound resilience |
≥ 40 % |
|
Service temperature |
−30 °C to +80 °C |
|
Fixing |
Pin and sleeve, bolt-through, or rail clamp |
Ordering
Send the bar spacing, deck outline, deck inclination and maximum lump size. Bar spacing is not the same as aperture width on a panel, so we convert it against your required cut rather than copying the number.
FAQ
MOQ is 10 pcs. Standard lead time is 15 days, and standard mold making takes 10 days.
Yes. Inclination is part of the specification — a steep deck needs a different land width and fixing layout from a horizontal one, so send the angle with the drawing.
Available as a custom tool. Above that size the land width becomes the design driver, and we will size it against your lump size and drop height.