A banana deck does three different jobs along its length, and one panel specification cannot do all three. The steep section at the feed end runs a thin, fast bed that strips fines almost immediately. The middle slope transitions. The shallow section at discharge runs a slow, thick bed where particles hover at the cut point for most of their travel — and that is where pegging happens.
Specifying panels for a banana screen therefore means specifying them by position.
Aperture graded to the slope. The feed-end section can carry a coarser aperture without losing product, because the bed is moving quickly and the fines have already separated. The discharge section, where the bed is slow and near-size material accumulates, needs the tapered slot geometry that releases rather than traps. Running one aperture across the whole deck is the most common reason a banana screen underperforms its rated capacity.
Thickness follows the load, not the catalogue. Impact governs the steep feed section, so 40 mm goes there. Sliding wear governs the shallow discharge section, where a 25–30 mm section lasts just as long and takes weight off the deck. Grading thickness this way usually reduces total panel cost without shortening service life anywhere on the deck.
Fixing that holds on a variable-slope frame. Banana decks change angle several times across the frame, and each transition is a place where a panel can lift and start to drum. Pin and sleeve fixing loads the panel along its length rather than at discrete bolt points, so the panel stays seated through the transitions.
Sealed edges at every cut line. A banana deck is built from panels of varying length. Each one is cut and edge-sealed at the factory to your drawing, so no slurry path opens into the frame at the joints between sections.
Banana and multi-slope screens in coal preparation, iron ore and base metal plants, phosphate and industrial mineral circuits, and any high-capacity fine separation deck where the slope changes along the machine.
| Item | Specification |
|---|---|
| Thickness | 40 mm standard; 25–60 mm on request |
| Panel size | Custom cut to your deck drawing |
| Aperture | 3–100 mm, slotted or square; tapered option |
| Hardness | Shore A 85 (75–95 available) |
| Compound | Hydrolysis-resistant wear grade polyurethane |
| Density | 1.10–1.15 g/cm³ |
| Tensile strength | ≥ 30 MPa |
| Tear strength | ≥ 80 kN/m |
| Abrasion (DIN 53516) | ≤ 40 mm³ |
| Rebound resilience | ≥ 40 % |
| Service temperature | −30 °C to +80 °C |
| Fixing | Pin and sleeve, bolt-through, or rail clamp |
Send the deck drawing with the slope angles and section lengths marked, plus cut point, feed gradation and tonnage. We return a drawing showing aperture and thickness by position, not a single specification for the whole deck.
What is your MOQ and lead time? MOQ is 10 pcs. Standard lead time is 15 days, and standard mold making takes 10 days.
Should every section of a banana deck use the same aperture? Rarely. The feed section usually runs coarser because the bed is thin and moving fast; the discharge section needs the tapered profile because that is where near-size material accumulates. Send the slope layout and we will grade the aperture accordingly.
Why does my banana screen peg on the last third of the deck? Because that is where the bed slows down and thickens. Near-size particles sit at the cut point with less energy to move them. A tapered slot plus a thinner, more flexible section at discharge is the usual fix.