Coke and Sinter Screen Panel in Polyurethane for Cooled Metallurgical Duty
Two things govern screening on the coke and sinter side of an ironworks: the material must reach the screen cooled, and it must arrive at the blast furnace in the size fraction it was graded into. Steel media handles the first requirement and undermines the second, because a hard, rigid deck degrades the product it is sizing.
Let us be clear about the limit first. Polyurethane on this panel family is rated for continuous service from −30 °C to +80 °C. Coke and sinter must be cooled to within that range before the deck. If your material arrives hotter, this is the wrong product and we will say so.
Less degradation of a friable product. Coke is graded, then handled, then graded again, and every hard impact makes fines that have no value in the furnace. An elastic polyurethane surface with rebound resilience at or above 40 % returns part of that impact energy, which measurably reduces degradation across the deck.
Abrasion resistance against sinter dust. Sinter fines are sharp, dense and carry a high dust load that works into any gap in the deck. A wear grade compound at ≤40 mm³ DIN abrasion holds the land width between apertures, which is what keeps the size fraction consistent over a campaign.
Slots that hold their dimension. The silent failure on a coke deck is a slot that has worn open, allowing oversize into a fraction that is sold on specification. A moulded slot keeps its width, so the product stays where it was specified rather than drifting over a season.
Fast change-out in a short window. Screening on the furnace feed side is maintained in tight windows. Pin and sleeve fixing lets a panel come off and go back on without bolting, which is what determines how much of the deck can actually be changed in one stop.
Where it runs
Coke screening and sizing after quenching and cooling, sinter plant cold screens, blast furnace feed sizing, and coke breeze and nut coke classification.
Technical data
| Item | Specification |
|---|---|
| Thickness | 40 mm standard; 25–60 mm on request |
| Panel size | Custom cut to your deck drawing |
| Aperture | 3–100 mm, slotted or square; tapered option |
| Hardness | Shore A 85 (75–95 available) |
| Compound | Hydrolysis-resistant wear grade polyurethane |
| Density | 1.10–1.15 g/cm³ |
| Tensile strength | ≥ 30 MPa |
| Tear strength | ≥ 80 kN/m |
| Abrasion (DIN 53516) | ≤ 40 mm³ |
| Rebound resilience | ≥ 40 % |
| Service temperature | −30 °C to +80 °C |
| Fixing | Pin and sleeve, bolt-through, or rail clamp |
Ordering
Send material type, temperature at the deck, size fractions required, tonnage and screen motion. Temperature at the screen is the first thing we check — if it is above 80 °C we will tell you before quoting rather than after.