Quick Link
Quick Contact
Address
No.367 Beijing Road, Longquanyi District, Chengdu, China
Tel
86--13981727059
Our Newsletter
Subscribe to our newsletter for discounts and more.
Tailings Dewatering Screen Panel in Polyurethane for Higher Solids Recovery
A tailings dewatering deck has one job and one number: how much water comes back and how much solid goes out with it. Every cubic metre of water that leaves with the tailings is water you have to replace, and every tonne of solid that reports to the return water is a problem you will meet again in the thickener.
Thin bed, high frequency, short residence time. Dewatering works by giving water a path out before the bed consolidates. That requires a thin, fast-moving bed on a deck with high acceleration and small amplitude. A light polyurethane panel suits that motion; a heavy steel or thick rubber deck loads the frame and forces a compromise on stroke.
Slots that stay open under the bed. The failure mode on tailings duty is not wear, it is progressive blinding at the discharge end, where the bed is driest and the fines are most concentrated. Tapered slots and panel flex release those particles on the return stroke, so the last third of the deck keeps draining instead of sealing over.
Low-friction surface releases water. Polyurethane sheds water more readily than rubber, so the film drains from the panel face rather than clinging to it. On a deck running at 0.25–0.5 mm slots, that surface behaviour is a measurable part of the final moisture figure.
Panel mass that suits the drive. A lighter deck lets the machine run higher acceleration at the same bearing load, and acceleration is the variable that actually moves water through a fine bed.
Where it runs
Tailings dewatering and recovery in coal, iron ore, copper, gold and mineral sands plants, plus backfill preparation and paste plant feed where solids recovery sets the downstream duty.
Technical data
|
Item |
Specification |
|
Thickness |
40 mm standard; 25–60 mm on request |
|
Panel size |
Custom cut to your deck drawing |
|
Aperture |
3–100 mm, slotted or square; tapered option |
|
Hardness |
Shore A 85 (75–95 available) |
|
Compound |
Hydrolysis-resistant wear grade polyurethane |
|
Density |
1.10–1.15 g/cm³ |
|
Tensile strength |
≥ 30 MPa |
|
Tear strength |
≥ 80 kN/m |
|
Abrasion (DIN 53516) |
≤ 40 mm³ |
|
Rebound resilience |
≥ 40 % |
|
Service temperature |
−30 °C to +80 °C |
|
Fixing |
Pin and sleeve, bolt-through, or rail clamp |
Ordering
Send feed solids content, particle size distribution, target cake moisture, deck dimensions and screen motion. If you are replacing an existing deck, send the moisture you achieve now — that is the baseline the change is judged against.