Steel Reinforced Polyurethane Dewatering Screen Panel Custom Cast for Wide Heavy Duty Decks
On a wide deck carrying a deep bed, the panel is not only a wear surface, it is a structural member. Under tension and load it either holds its plane or it takes a set, and a panel that has taken a set drains unevenly across its width for the rest of its life. Steel reinforcement inside the casting is what keeps the geometry where it was moulded.
Steel insert cast into the panel. A steel reinforcing frame is bonded inside the polyurethane during casting, so the panel resists bending and tension across the span rather than relying on the compound alone. The insert is fully encapsulated and does not see the slurry.
Plane held over a long campaign. A deck that stays flat drains the same at the side plates as it does in the middle. A panel that deflects between support rails passes a wetter band down one side, which typically shows up as an unexplained moisture variation rather than as a visible fault.
Built for deep beds and heavy feed. Where the bed is deep and the feed is coarse, the load on the panel face is high and the wear is concentrated. The reinforced casting takes that load without adding support rails to the deck.
Custom cast, not cut from sheet. Each panel is cast to your drawing, so the reinforcement layout follows the panel outline and the fixing positions. Cut-outs and asymmetric panels are reinforced where they need it rather than uniformly.
Where it runs
Heavy duty primary dewatering, ROM and coarse tailings decks, wide decks with widely spaced support rails, and high tonnage coal or mineral installations where panel deflection has been a problem.
Technical data
|
Item |
Specification |
|
Thickness |
40 mm standard; 25–60 mm on request |
|
Panel size |
1044 mm x 702 mm standard; custom cut to your deck drawing |
|
Aperture |
0.1–100 mm slotted or square; tapered option |
|
Hardness |
Shore A 85 (75–95 available) |
|
Compound |
Hydrolysis-resistant wear grade polyurethane |
|
Density |
1.10–1.15 g/cm³ |
|
Tensile strength |
≥ 30 MPa |
|
Tear strength |
≥ 80 kN/m |
|
Abrasion (DIN 53516) |
≤ 40 mm³ |
|
Rebound resilience |
≥ 40 % |
|
Service temperature |
−30 °C to +80 °C |
|
Fixing |
Pin and sleeve, bolt-through, or rail clamp |
Customisation
The reinforcement layout is set for the load case on your deck: support rail spacing, bed depth and feed size all go into the drawing before the insert is formed. Panel outline, cut-out positions and fixing holes are cast to your drawing, and asymmetric or edge panels are reinforced where the load actually is.
Ordering
Send the deck drawing, the support rail spacing, the bed depth and the feed size. If panels have deflected or cracked in service before, send photos of the failure so the reinforcement layout can be set for that load case.
FAQ
Will the steel insert corrode?
The insert is fully encapsulated in polyurethane during casting, so it is not exposed to slurry or wash water. Damage that exposes it is visible and the panel should then be replaced.
Is a reinforced panel heavier to handle?
Yes, marginally heavier than an unreinforced panel of the same size. Where panels are changed by hand, tell us and we will confirm the handling weight on the drawing.
Can reinforced panels be cut on site?
No. The insert has to be allowed for at casting, so any cut-out or edge shape must be on the drawing before the panel is made.