Fine Sand Recovery Screen Panel in Polyurethane for Cyclone Underflow
In a sand plant, the fines that get away are the cheapest product you will ever lose. A conventional sand screw recovers down to about 0.15–0.2 mm and lets the rest report to the settling pond, where it becomes a dredging cost instead of a sale. A fine sand recovery screen sits on the cyclone underflow and takes that fraction back.
High frequency, small amplitude, thin bed. Fine sand recovery depends on acceleration rather than on residence time. The deck runs at high frequency with a shallow bed so water is thrown off the surface before the layer consolidates. A light polyurethane panel is the natural match for that motion.
Slots specified at the cut, tapered to stay open. On 0.1–0.3 mm duty, blinding is the whole game. Tapered slots open through the panel thickness, and the panel flexes under the high-frequency stroke, so near-size particles release instead of sealing the deck within an hour of start-up.
Recovers product, not just water. A recovery deck that blinds does not fail visibly — it just starts sending fines back to the pond. Checking the underflow gradation monthly is how you catch a deck that has quietly stopped recovering.
Weight that suits a high-frequency drive. High-frequency units are sensitive to moving mass. Keeping the panel section thin and light is what lets the drive run at its design frequency rather than at whatever the deck mass allows.
Where it runs
Fine sand recovery behind cyclones in sand and gravel plants, manufactured sand lines, silica sand, mineral tailings recovery and dredging spoil processing.
Technical data
|
Item |
Specification |
|
Thickness |
40 mm standard; 25–60 mm on request |
|
Panel size |
Custom cut to your deck drawing |
|
Aperture |
3–100 mm, slotted or square; tapered option |
|
Hardness |
Shore A 85 (75–95 available) |
|
Compound |
Hydrolysis-resistant wear grade polyurethane |
|
Density |
1.10–1.15 g/cm³ |
|
Tensile strength |
≥ 30 MPa |
|
Tear strength |
≥ 80 kN/m |
|
Abrasion (DIN 53516) |
≤ 40 mm³ |
|
Rebound resilience |
≥ 40 % |
|
Service temperature |
−30 °C to +80 °C |
|
Fixing |
Pin and sleeve, bolt-through, or rail clamp |
Ordering
Send cyclone underflow gradation, target recovery size, feed solids, deck dimensions and unit frequency. Recovery size and slot size are not the same number; we size the slot against the gradation you send.
FAQ
What is your MOQ and lead time?
MOQ is 10 pcs. Standard lead time is 15 days, and standard mold making takes 10 days.
What is the finest particle a recovery screen can hold?
Practically around 0.075–0.1 mm on a well-set deck, and the limit is set by surface tension as much as by the slot. Below that, the water film carries the particle through regardless of aperture.
How often should the deck be checked?
Monthly underflow gradation is enough to catch progressive blinding, plus a visual check of the discharge end each shift — that is where blinding shows first.