Ultra Fine Dewatering Panel in Polyurethane with Slots Down to 0.25 mm
Below half a millimetre, dewatering stops being a mechanical process and becomes a surface physics problem. Water does not flow through a 0.25 mm slot the way it flows through a 2 mm one — capillary forces hold it, surface tension bridges it, and the boundary layer on the panel face is thick enough to matter.
Slot tolerance is the whole specification. At 0.25 mm, a 0.03 mm variation is a 12 % change in open area, and on a production panel that is the difference between draining and blinding. Slots are moulded from a machined tool rather than cut, so the width is consistent across the panel and between panels.
Taper to break the capillary hold. A straight-walled fine slot holds water by capillary action at the exit. A taper gives the water film a diverging path, which is what allows it to break away instead of sitting in the slot. This is the detail that makes a fine slot work rather than merely exist.
Thin section for higher acceleration. Fine dewatering runs best on a light panel at high frequency and small amplitude. A 15–25 mm section suits that motion and keeps the moving mass within what the drive was designed for.
Surface energy that releases the film. Polyurethane's lower affinity for water is a real advantage at fine apertures, because the water film leaves the surface instead of clinging to the land between slots.
Where it runs
Fine coal and mineral tailings dewatering, starch and chemical processing, food and pharmaceutical solids recovery, and industrial effluent polishing where solids carry-over is regulated.
Technical data
|
Item |
Specification |
|---|---|
|
Thickness |
40 mm standard; 25–60 mm on request |
|
Panel size |
Custom cut to your deck drawing |
|
Aperture |
3–100 mm, slotted or square; tapered option |
|
Hardness |
Shore A 85 (75–95 available) |
|
Compound |
Hydrolysis-resistant wear grade polyurethane |
|
Density |
1.10–1.15 g/cm³ |
|
Tensile strength |
≥ 30 MPa |
|
Tear strength |
≥ 80 kN/m |
|
Abrasion (DIN 53516) |
≤ 40 mm³ |
|
Rebound resilience |
≥ 40 % |
|
Service temperature |
−30 °C to +80 °C |
|
Fixing |
Pin and sleeve, bolt-through, or rail clamp |
Ordering
Send the particle size distribution, feed solids content, target solids carry-over and deck motion. On ultra-fine duty the gradation decides whether a slot panel works at all, so we will check it before quoting.