Frac Sand Dewatering Panel in Polyurethane for Washed 20/40 and 40/70 Product
In a frac sand plant, the dryer is the largest single energy cost after the mining itself. Every percentage point of moisture that reaches the dryer has to be boiled off, and at 200 tph that is a number large enough to justify a serious look at what happens on the dewatering deck upstream.
Deck performance sets dryer load. The dewatering screens ahead of the dryer are the last chance to remove free water cheaply. A deck that is blinded at the discharge end passes a wetter product to the dryer, and the cost shows up in gas consumption rather than in a screening complaint.
Slots specified for the product band. Frac sand is a narrow, tightly specified product band, and the slot has to retain the fine end of that band while draining fast. Slots are moulded to the cut and held to tolerance, so the deck retains the same fraction at the end of a campaign as at the start.
Angular grains drain differently from round ones. Crushed frac sand holds water in the interstices of the bed more than rounded natural sand does. That makes bed depth control and panel flex more important than slot size alone on this duty.
Stable geometry over a long campaign. Frac sand plants run continuously, and a deck that takes a set or deflects over the support rails will drain unevenly across its width. A panel that holds its plane keeps the moisture figure consistent from one week to the next.
Where it runs
Wet frac sand plants, hydraulic fracturing proppant production, resin-coated sand feed preparation, and silica sand washing where moisture ahead of drying is the cost driver.
Technical data
|
Item |
Specification |
|
Thickness |
40 mm standard; 25–60 mm on request |
|
Panel size |
Custom cut to your deck drawing |
|
Aperture |
3–100 mm, slotted or square; tapered option |
|
Hardness |
Shore A 85 (75–95 available) |
|
Compound |
Hydrolysis-resistant wear grade polyurethane |
|
Density |
1.10–1.15 g/cm³ |
|
Tensile strength |
≥ 30 MPa |
|
Tear strength |
≥ 80 kN/m |
|
Abrasion (DIN 53516) |
≤ 40 mm³ |
|
Rebound resilience |
≥ 40 % |
|
Service temperature |
−30 °C to +80 °C |
|
Fixing |
Pin and sleeve, bolt-through, or rail clamp |
Ordering