Clay in the feed does not wear a panel out. It shuts a plant down gradually. A wet, plastic clay fraction smears across the panel face, bridges the slots, and takes open area away a little at a time. Throughput drops, the operators add water, the added water carries more fines away, and the plant ends up both slower and losing product.
Tapered slots break the smear. Every slot widens through the panel thickness rather than running straight-walled, so material that enters cannot stand at mid-depth. That geometry, rather than slot size, is what keeps a clay-bound feed draining.
Panel flex breaks the bridges. At 25–40 mm, the section deflects under the deck and returns, and that movement is what releases material spanning a slot. Rigid media — punched plate, wedge wire — cannot do this, which is why the same feed behaves differently depending on what it is running on.
Open area prioritised over land width. On sticky duty, a smaller open area is a bigger liability than reduced wear life, because a blinded deck has no throughput at all. We size land width against your clay load rather than maximising wear life on paper.
Wash water used deliberately. Adding water helps up to a point, and past that point it costs you fines. Tell us what you are currently adding and we will tell you whether the panel layout or the water practice is the thing to change first.
Pit sand with clay bands and seams, weathered mountain sand, excavation arisings, excavation material from construction sites and any feed where blinding rather than wear sets the throughput ceiling.
| Item | Specification |
|---|---|
| Thickness | 40 mm standard; 25–60 mm on request |
| Panel size | 500 x 550 mm standard; custom cut to your drawing |
| Slot width | 0.1–4.0 mm slotted; tapered option |
| Slot tolerance | ±0.03 mm on slot width |
| Open area | 20–38 % depending on slot width |
| Hardness | Shore A 85 (75–95 available) |
| Compound | Hydrolysis-resistant wear grade polyurethane |
| Density | 1.10–1.15 g/cm³ |
| Tensile strength | ≥ 30 MPa |
| Tear strength | ≥ 80 kN/m |
| Abrasion (DIN 53516) | ≤ 40 mm³ |
| Rebound resilience | ≥ 40 % |
| Service temperature | −30 °C to +80 °C |
| Fixing | Bolt-through, pin and sleeve, or rail clamp |
Send a feed description — clay content, plasticity if you know it, moisture and gradation — plus the machine drawing. On sticky duty the feed description matters more than the tonnage, so please be specific rather than approximate.