Sea sand is the hardest washing duty in the industry, for a reason that has nothing to do with the sand. Chloride is corrosive to nearly every metal in a plant, including stainless grades that are supposed to handle it. A component that lasts three years inland can fail inside one year here, and the failures are rarely gradual.
Salt water does not attack the panel. Polyurethane is not susceptible to chloride attack in the way the frame, bolts and surrounding steelwork are. On a plant where everything else corrodes, the screen panel tends to outlast the structure around it.
Fine slots stay dimensionally stable. Desalination washing separates at fine cuts, typically 0.2–0.5 mm, and the whole point is that every particle gets the same exposure to wash water. Slot tolerance of ±0.03 mm and a wear-resistant compound mean the separation does not drift as the panel ages.
Handles shell fragments without damage. Sea sand carries shell, which is hard, brittle and plate-shaped. Shell fragments are hard, brittle and plate-shaped. A flexible polyurethane section lets that material pass and deflect rather than taking the impact rigidly, which is why shell does less damage here than it does on a punched plate or wedge wire panel.
Wet continuously, and it does not matter. Salt water, continuous immersion and sunlight are the conditions in which standard elastomers swell and soften. The compound is a hydrolysis-resistant grade specified for permanent wet service, so the panel behaves the same after a year as it did at commissioning.
Where it runsSea sand desalination and washing plants, dredged marine sand processing, beach sand recovery operations and coastal aggregate plants handling chloride-bearing feed.
Technical data| Item | Specification |
|---|---|
| Thickness | 40 mm standard; 25–60 mm on request |
| Panel size | 500 x 550 mm standard; custom cut to your drawing |
| Slot width | 0.1–4.0 mm slotted; tapered option |
| Slot tolerance | ±0.03 mm on slot width |
| Open area | 20–38 % depending on slot width |
| Hardness | Shore A 85 (75–95 available) |
| Compound | Hydrolysis-resistant wear grade polyurethane |
| Density | 1.10–1.15 g/cm³ |
| Tensile strength | ≥ 30 MPa |
| Tear strength | ≥ 80 kN/m |
| Abrasion (DIN 53516) | ≤ 40 mm³ |
| Rebound resilience | ≥ 40 % |
| Service temperature | −30 °C to +80 °C |
| Fixing | Bolt-through, pin and sleeve, or rail clamp |
Send chloride content if measured, shell content, target residual chloride in the product, tonnage and machine drawing. If you have had premature failures of panels or hardware before, tell us what failed first — it usually identifies the real problem.